While it has been good to see the colour changes that can happen when applying heat to the iron based ochres, this controlled fashion has limits for me. Without pushing things I can get the pigment samples up to about 1100 °C (roughly 2000 °F) and this gets me well into the brown range of colour.
But, if pushed further, the iron rich earths should go a dark purple, and then black. While I can’t control or measure the temperature in this process, as an artist I’ll just state that it’s, “really” hot. The pigment sample was bright yellow during the heating, if that gives any indication.
I’ll share the results when it cools down!
Related posts:
- Firing Conestoga Pigments
With the pigment from the Conestogo river collected and purified I began to test the effects of heating in earnest. Increasing the temperature by 100ºF... - Nova Scotia Pigments
It has been 9 months since my brother, Aaron, and I spent the week collecting pigment/rock samples from old mines in Nova Scotia and the... - Cone 10 Pigments
When I saw the sign in the window of S & S Pottery Supplies asking for fill in an upcoming cone 10 gas firing I...